MIL-STD-2219A
w/CHANGE 1
TABLE lll. Shielding gas and material combinations.
Material |
Gas 1/ |
||||||
Argon |
Helium |
Argon Helium |
Argon 2/ Oxygen |
Argon Hydrogen |
Nitrogen |
Carbon Dioxide |
|
Aluminum |
A |
A |
A |
||||
Cobalt |
A |
A |
A |
A |
|||
Copper |
A |
A |
A |
||||
Magnesium |
A |
A |
A |
||||
Nickel |
A |
A |
A |
||||
CRES Steels |
A |
A |
A |
A |
Backing only |
||
Plain Carbon Steels |
A |
A |
A |
A |
3/ |
||
Low alloy Steels |
A |
A |
A |
A |
|||
Titanium |
A |
A |
A |
Notes:
A = Allowed
1/ Gas compositions and mixtures shall comply with TABLE I.
2/ 8 percent oxygen maximum.
3/ Only permitted on plain carbon steel with a maximum of 0.25 percent nominal carbon.
5.3.5.8 Post weld cleaning
Except as noted in 5.4.4.3 and 5.4.4.4, completed weldments shall be free of visible oxides, flux, spatter, scale, slag, or other foreign matter. Cleaning, if required, shall be in accordance with 5.2.2.2. Welding flux shall be completely removed by appropriate methods. Removal of material during the cleaning operation shall not exceed the allowed tolerances of the end product specification.
5.3.6 Stress relief
When required, stress relief of weldments shall be specified in the welding procedure or the drawing.